Software Downloads

Software Downloads & Support TA Instruments strives to deliver high quality software products. These products are continuously updated to add features, support new instruments, and repair software issues. In addition, your input regarding our software products is important to us. Software Downloads Links TRIOS SoftwareNano Series SoftwareTAM Assistant Series SoftwareAdvantage/UA SoftwareSA+ SoftwareWinTest SoftwareWinTest DMA SoftwareScarabaeus SoftwareOrchestrator…

DSC Step Annealing for Fingerprinting Molecular Structure in Poly(vinylidene fluoride)

DSC step annealing is used to study the fine molecular structure of poly(vinylidene fluoride) (PVDF) homopolymers and copolymers. The melting pattern, obtained after step annealing, is a characteristic “fingerprint” for small variations in structure. This “fingerprint” detects variations in the polymerization process, the molecular weight of the polymer, the fraction and the nature of the co-monomer.

Simple Determination of the Linear Viscoelastic Region of a Polymer Using a Rheometer

Materials such as polymers exhibit viscoelastic behavior which is directly related to molecular structure and formulation differences. To accurately evaluate the relationships between molecular structure and viscoelastic behavior requires that experiments, such as rheological measurements, be conducted in regions where the viscoelastic properties observed are independent of imposed stress or strain levels. That is, experiments must be conducted in the linear viscoelastic region.