Gasification of Waste Materials and Coal in High Pressure TGA
A lignite coal sample and several petroleum coke samples have been gasified in the new Discovery HP-TGA 75 and 7500 instruments using carbon dioxide and steam as gasifying agents. The evolved gas atmosphere was analyzed with online mass spectrometry to detect the generated syngas components.